應(yīng)用 Applications
這種類型的設(shè)備,適應(yīng)的物料比較多,除基本型提及的物料外,還有:.A.B.C中間體、A.B.S樹脂、A.S.C、 白碳黑、苯茶毗酮、茶粕、草酸催化劑、促進(jìn)劑m、d.m、觸媒、沉淀炭粉、對乙酷氮基苯磺酷氨、、哆耳瑪托、對苯二酸、二乙苯按、二氧花、活性碳、氟硅酸鈉、 氟石礦、副產(chǎn)硫按、硅膠粉末、合成樹脂、磺酸鈣、 聚丙烯樹脂、、焦硅酸鈉、糠氯酸咖啡渣、、硫酸鈉、硫化礦、磷礦粉、蘭BB、P.V.C、熔融磷肥、 四環(huán)素、三氧化鐵、碳酸鈣、欽鐵礦、銅礦、土豆粉、尾煤、硬脂酸鹽、玉米蛋白、藥品、藥劑、氧化鐵、酒渣等。
This type of equipment is suitable for many materials, except those mentioned in the basictype. Also: methaqualone, A.B.C intermediate, A.B.S resin, AS.C, white carbon blackbenzene-tea pyrazolone, tea meal, oxalic acid catalyst, accelerant m, d.m, catalyst.precipitated carbon powder,p-acetylazobenzene sulfony ammonia, p-aminosalicylic acidtolmetol, p-phenylene diacid, diethylbenzene ammonium, titanium dioxide, activated carbon.sodium fluosilicate, fluorspar ore, byproduct ammonium sulfate, silica gel powder, syntheticresin, calcium sulfonate, polypropylene resin, aureomycin, Sodium pyrosilicate, bran chloricacid coffee residue, oral glucose, sodium sulfate, sulfide ore, phosphate rock powder, blueBB, PV.C. molten phosphate fertilizer, tetracvcline, ferric oxide, calcium carbonate, ilmenitecopper ore, potato powder, tail coal, stearate, zein, drugs, pharmaceuticals, iron oxide, wineresidue,etc.
原理 Principles
具有分散作用的風(fēng)機(jī),特別適合熱敏性物料的氣流干燥作業(yè)。高速飛旋的風(fēng)機(jī)葉輪,能把濕的、甚至結(jié)塊的物料解碎,直至分散,在分散過程中同時攪拌、混合,然后物料和熱氣流平行地流動。這種類型的設(shè)備,適應(yīng)干燥濾餅結(jié)塊的,但還屬于表面水份的物料,含濕量≤40%,如果處理量大或者成品要求干至15%以下時,可采用二級氣流干燥。當(dāng)物料含濕量超過40%,但<60%時,進(jìn)料較困難,應(yīng)采用混料器,通過混進(jìn)干料的方法以降低進(jìn)料水份,此時,干燥設(shè)備的總產(chǎn)量就有較大幅度的下降,這在經(jīng)濟(jì)上是不合算的。因此,用戶應(yīng)先用機(jī)械的方法(離心脫水或壓濾)盡可能的降低進(jìn)料水份,以確保干燥作業(yè)上的順利進(jìn)行。
Fan with dispersing function is especially suitable for airflow drying of heat sensitivematerials.The high-speed whirling fan impellercan break up wet or even cakedmaterials until they are dispersed,stir and mix atthe sametime during the dispersionprocess, and then the materials and hot air flow in parallel.This type of equipment issuitable for drving materials with caked filter cakes, but also with surface moisturecontent less than or equal to 40%. if the treatment capacity is large or the finishedproduct requires drying below 15%, secondary air flow drying can be adopted. Whenthe moisture content of the material exceeds 40%, but is less than or equal to 60%, itis more difficult to feed. A mixer should be used to reduce the moisture content of thefeed by mixing dry materials. At this time. the total outout of the drving eauipment wll be greatly reduced, which is uneconomical, Thereforeusers should first use mechanical methods (centrifugal dehydration or pressure flktration) to reduce the feed water as much as possible toensure the smooth progress of drving operations.
技術(shù)參數(shù) Technicalparameters
型號 | 蒸發(fā)水份(kg/h) | 裝機(jī)功率(kw) | 占地面積(㎡) | 高度(m) |
QG 50 | 50 | 10 | 20 | 9 |
QG 100 | 100 | 20 | 32 | 11 |
QG 200* | 200 | 31 | 40 | 11 |
QG 250 | 250 | 32 | 64 | 13 |
QG 500 | 500 | 54 | 96 | 13 |
QG 1000* | 1000 | 135 | 120 | 15 |
QG 1500* | 1500 | 175 | 200 | 16 |
干燥實例 Dried samples
物料名稱 | 進(jìn)料混含量 | 產(chǎn)品濕含量% | 風(fēng)進(jìn)口溫度/℃ | 廢氣排出溫度/℃ | 產(chǎn)品粒數(shù)/日 |
阿斯醫(yī)林 | 2.5-5 | 0.2 | 80 | 60 | |
玫瑰精 | 35 | 3-4 | 180 | 60 | 40 |
草酸 | 4-5 | 0.5 | 120 | 40 | 20 |
醋酸鈉 | 10 | 2-3 | 80-90 | | |
味精 | 4-5 | 0.1 | 100 | | |
藥用小蘇打 | 3 | 0.05 | 110 | | |
焦亞硫酸鈉 | 5-6 | 0.05 | 100 | 40 | |
葡萄糖 | 16-17 | 9.1 | 90 | 40 | 20日 |
小麥淀粉 | 40-41 | 12-14 | 240-260 | 50-55 | |
明砂 | 4-5 | 0.5 | 70-90 | 50 | |
玉米淀粉 | 40 | 13 | 120-130 | 40 | 80-100日 |
NH.HCO | 6 | 0.5以下 | 70-90 | 50 | |
硬脂酸鹽類 | 40-50 | | 105-200 | 70-80 | 200 |
氟硅酸鈉 | 12 | 1以下 | 400 | 160 | |
苯甲酸 | 25 | 0.5 | 110 | 60 | 80 |
六六六 | 12-14 | 5-6 | 90 | 40-50 | |
吡唑酮 | 15 | 0.6 | 90-110 | 55-60 | |
堿化煤 | 60-70 | 20-40 | 250進(jìn)口 | | |
硫銨 | 1.8-2.5 | 0.02-0.08 | 110-115 | 70-90 | |
磺酸(SN) | 20 | 1 | 110-120 | 50 | 1.5 |
對氨基粉 | 10 | 0.4 | 240 | 70 | |
淀粉 | 42.9 | 12.7 | 147.6 | 38.2 | 0.05 |
活性炭 | 205 | 4 | 455 | | |
熔融磷胞 | 5 | 0.3 | 200 | | |
茶箱 | 115 | 6.4 | 620 | | |
促進(jìn)劑M.D.M | 20 | 0.5以下 | 150 | 50-80 | 100 |
6-7 | 0.2 | 135-140 | 75-80 | 40-60 | |
鋸別 | 77 | 50 | 220 | 60 | 粒狀 |
安乃通 | 20 | 4-5 | 100 | 70 | |
聚甲醛 | 20 | 1 | 135 | 65 | 120-150 |
食用小蘇打 | 3.9 | 0.2 | 180-240 | 50-70 | 0.005-0.001mm |
微球催化劑 | 25 | 13 | 500-580 | 130-150 | 40-50 |
717離子交換樹脂 | 4-7 | 0.1-0.4 | 120 | 70-80 | 1-200 |
觸媒 | 18-25 | 5 | 110-130 | 60 | 18-20 |
次亞硫酸鈉 | 5.8 | 0.2 | 150 | 108 | |